Optical Grade LiTaO3(LT) Wafer
LiTaO3 crystal is also widely used E-O crystal, due to its optical, NLO and E-O poperties similar to those of LiNbO3 crystal, but with higher damage threshold (> 500 MW/cm2 for ns pulsed).
Applications
1 ) Quasi-phase Matching for SHG and OPO 2 ) Pyroelectric Infrared Detector
Specifications
Material | Optical Grade LiTaO3 crystal | |
Curie Temp | 603±2℃ | |
Cutting Angle | Z-cut etc | |
Diameter/size | 3”/4” | |
Tol(±) | <0.20 mm | |
Thickness | 0.18 ~ 0.5mm or more | |
Primary Flat | 22mm /32mm | |
TTV | <3µm | |
Warp | <40µm | |
Surface Type | Single Side Polished /Double Sides Polished | |
Polished side Ra | <0.5nm | |
Back Side Criteria | General is 0.2-0.5µm or as customized | |
Edge Criteria | R=0.2mm or Bullnose | |
Optical doped | Zn/MgO etc | |
Wafer Surface Criteria | Contamination, | None |
Particles ¢>0.3 µ m | <= 30 | |
Scratch , Chipping | None | |
Defect | No edge cracks, scratches, saw marks, stains | |
Packaging | Qty/Wafer box | 25pcs per box |